Figure 5.

Comparison of cumulative iron concentration as a function of time for 63–75 μm splits of pyrite HY-001 produced by different grinding methods: hand grinding using an agate mortar and pestle vs. machine grinding using a mixer mill. In both cases, the ground samples were wet sieved.

Wolfe et al. Geochemical Transactions 2007 8:9   doi:10.1186/1467-4866-8-9