Figure 3.

Adenine exposed to varying pyrite particle loadings (without the addition of hydrogen peroxide). Adenine concentrations were determined by measuring absorbance at 260 nm from filtered samples.

Cohn et al. Geochemical Transactions 2010 11:2   doi:10.1186/1467-4866-11-2